ADMET Foam Testing Systems
ADMET's easy to use and highly accurate universal testing machines are commonly used by the foam industry to test the indentation / compression force deflection (IFD & CFD), tensile, and tear strength properties of all types of foams. ADMET's testing systems will perform your foam tests according to ASTM or ISO standards.
Common foam tests:
1. Indentation Force Deflection Test (IFD) - Specified Deflection
2. Indentation Force Deflection Test (IFD) - Specified Force
3. Compression Force Deflection (CFD)
4. Tension Test
5. Tear Resistance Test
Dual column testing machines such as our eXpert 2600 series can perform IFD, CFD, tension, and tear tests. Our smaller single column eXpert 7600 series of testing machines are perfect for performing tension and tear tests as well as compression testing on smaller samples. To learn about all of the equipment requirements for foam testing, please click here.
The following videos show a few common foam tests. If you would like more information about each specific test, use the link below each video.
Read more about the foam tensile strength test
Read more about the ASTM D3574 foam IFD test
Read more about the foam tear strength test