How to Perform an ASTM C469 Concrete Compression Test

  
  
  
  
  
ASTM C469 governs the determination of static Modulus of Elasticity and Poisson's Ratio of concrete in compression.  The ensuing video demonstrates a C469 test on a hydraulically actuated manually controlled Baldwin universal testing machine equipped with an ADMET Gauge Buster 2 Digital Indicator and a computer running ADMET's Gauge Safe Live Data Exchange program.  The digital indicator and computer are connected via a USB port. 
 
 
 
ASTM C469 Test 
Figure 1 - Depiction of ASTM C469 Test Setup with Gauge Buster 2 Digital Indicator and Compressometer equipped with axial and transverse strain measuring transducers. 
 
For more information, please visit our CONCRETE TESTING webpage. 