Rubber Seal Compression Testing to Obtain Load vs. Deflection Curve
Posted on Fri, Mar 26, 2010 @ 12:11 PM
This video shows a compression test on a rubber door seal to obtain the load vs. deflection curve and to determine the load at various displacements. For example, our customer wanted to know the load at 5, 15, and 30% compression of the original height. The zero point on the X (displacement) axis was set for the design height. Load on the chart before or after the zero point would indicate manufacturing tolerance- either the seal was produced too large or too small.
All ADMET testing systems are fully customizable. If you have any questions regarding an application or system, please call 800-667-3220, email info@admet.com, or fill an Ask an Engineer form.