Contact us

Call us: (800) 667-3220

Email us: info@ADMET.com

Ask an Engineer form

Request a quote form

Receive an email when a new video is posted

Your email:

About ADMET

  • Founded by engineers in 1989.
  • Offers advanced materials and product testing systems that are reliable and easy to use.
  • Willing to modify our systems to meet your needs.
  • On-site service and calibration team includes over 100 individuals in over 40 locations.
  • On-site and web based training.
  • Unlimited phone and email support.

Authors

Richard Gedney, Founder

Orick Kelley, Sales Engineer for metals, concrete, etc...

Debbi Cohen, Sales Engineer, medical materials and finished device testing applications

Andrew DeWolfe, Sales Engineer for plastics, foam, textiles, etc...

Current Articles | RSS Feed RSS Feed

Needle Syringe Test on a Universal Testing Machine

  | Share on Twitter Twitter | Submit to Digg digg it |  Add to delicious  delicious |  Submit to StumbleUpon StumbleUpon |  Share on LinkedIn LinkedIn | Submit to Reddit reddit 
 
Many different types of testing profiles can be used to test a syringe. There are ASTM and ISO standards, for example, ISO7864 and ISO9626, as well as individual company specified testing profiles. You may want to discover how much force it takes the press the plunger with and without liquid, or you may want to determine how easy or difficult the luer lock is to remove or to connect, or you may want to examine the pressure of the liquid when forced out of the syringe at a high speed, and more. In this example, we filled a syringe with a needle hub attached by luer lock with water. We compressed the plunger through its 1.75 inches of travel.  We were interested in measuring the average force required to push the fluid through syringe.  To obtain an accurate load average measurement, we needed to ignore the "noise" at the beginning and end of the stroke.  We programmed our machine to average the load between 0.5 - 1.5 inches of displacement.  This syringe test was performed on an ADMET eXpert 7601, Single Column, 1kN testing system equipped with an eP Digital Controller and a syringe testing fixture. This test gave us information on the force required to compress the plunger to a certain position. 
 
The test profile is as follows;
  • Preload to .01 lbs
  • Compress syringe plunger 1.5 inches
  • Measure Average Load and Peak Force
  
 
 