Sewn Seam Strength Test
Posted on Tue, Dec 29, 2009 @ 05:18 PM
Two pieces of nonwoven fiber joined at the edges by sewn thread are pulled apart at a constant rate of speed to measure the maximum peak force of the seam. Video below: