Plastic Bend Flexural Test
Posted on Mon, Nov 30, 2009 @ 01:43 PM
This video shows a plastic bend test similar to ASTM D790. This test was performed on our eXpert 7601 single column universal testing machine and our eP digital controller.
All ADMET testing systems are fully customizable. If you have any questions regarding an application or system, please call 800-667-3220, email info@admet.com, or fill an Ask an Engineer form.