Catheter Tubing Tensile Strength Test
Posted on Fri, Dec 18, 2009 @ 12:22 PM
This test stretches plastic medical catheter tubing until it fractures to measure its maximum elongation and tensile strength. We used our high elongation / low force eXpert 7601 single column testing machine equipped with a pair of bollard grips that are designed to hold tubular and cord type products in tension tests without creating premature breakage caused when using standard vise or wedge grips.