Packaging with Sugar Cane Plastic
Posted by Nicholas Schaulsohn on Mon, Mar 14, 2011 @ 08:23 AM
From Business Green - Sugarcane is harvested to produce sugar, which is then fermented and distilled to produce ethanol
. The ethanol is then dehydrated to create ethylene, which is polymerized into the final Plant-astic product...