Micro EP Used for Micro Tensile Testing of Plant Fibers
Posted by Nicholas Schaulsohn on Fri, Mar 25, 2011 @ 09:47 AM
We recently worked with a leading research university that needed a system to test the tensile properties of plant fibers. Scientists at the university required a system that was capable of holding small wood fibers and testing them at extremely low forces. The testing system also needed to be compatible with a video microscope and had to be able to perform tests inside a liquid bath.
The Micro EP is designed to work with microscopes, so a modified version of the system was a logical choice for this application. We equipped a Micro EP with an extremely low-capacity waterproof load cell designed to measure forces under 50 grams. The system was extended to accommodate an attachable bath and submersible fixtures, allowing the system to test samples in and out of liquid environments.
The university developed their own clamping mechanism, so we tested the system by conducting low-force tension fatigue tests on small rubber rings. The system was paired with ADMETs software-based MTESTQuattro controller. MTESTQuattro makes setting up complex test profiles easy and automatically calculates virtually every mechanical property, including: tensile strength, tensile stress and displacement.
This is just one of the many uses our customers have found for the Micro EP. In the past, ADMET has developed Micro EP’s to test solar films, biomedical tissue, and even perform tests in temperature chambers.

Standard Micro EP (left)and Extended EP with Bath (right)
Useful Links
Micro EP Testing System
ADMET Tensile Testing Solutions
ADMET Biomedical Testing Solutions
All ADMET testing systems are fully customizable. If you have any questions regarding an application or system, please call 800-667-3220, email info@admet.com, or fill an Ask an Engineer form.