How to set up an ASTM D1894 Test on an eP2 controlled Testing System
Posted by Andrew DeWolfe on Mon, Nov 07, 2011 @ 01:52 PM
If you seek to learn about the ASTM D1894 coefficient of friction test (COF), please read this article. This page assumes you understand the test and you already own an ADMET universal testing machine and COF fixture. If your machine came preloaded from the factory with the COF test method installed, you can skip the "how to program" video. Good luck, and call us should you have any questions.
How to perform the ASTM D1894 test method:
How to program the ASTM D1894 test method into the eP2 digital controller: