Posted by Andrew DeWolfe on Mon, Aug 29, 2011

The floating roller peel test is one of many types of tests designed to measure the average peel force of an adhesive or other bonding agent. The other common peel tests are the 90 degree, 180 degree, and T-Peel. Although not suitable for every application, the floating roller is a very accurate and easy method to obtain average peel force values.
Read More
Posted by Debbi Cohen on Mon, Aug 22, 2011

This is a summary and how to guide for ASTM F543 Standard Specification and Test Methods for Metallic Bone Screws.
Read More
Posted by Debbi Cohen on Wed, Aug 10, 2011
For over twenty years, ADMET has been designing state of the art testing systems for a range of industries. From plastics and adhesives to ceramic and metals, ADMET has established itself as a standard bearer in the world of material and device testing.
Read More
Posted by Debbi Cohen on Fri, Jul 29, 2011
Bone screws are designed to be inserted into bone or bone-like material to stabilize the area. The screws are subjected to different loads as the body moves and as the bones heal. This standard specification is used to determine how much force is required to cause a failure, either a break or removal, from the bone material. This method is used to compare uniformity of different screws.
Read More
Posted by Debbi Cohen on Tue, Jul 19, 2011
Small titanium, plastic, ceramic, and composite parts are crucial to the assembly of medical devices, medical parts for orthopedics, and dental devices. Many ASTM and ISO standards outline the test procedures and sample preparation. There are many references on the ADMET blog site.
Read More
Posted by Debbi Cohen on Wed, Jul 06, 2011

Why is this important? Companies and Universities spend R & D dollars testing various adhesives to determine which one will adhere to skin, but not be painful to remove.
Read More
Posted by Debbi Cohen on Wed, Jun 01, 2011

Dental composite resins are types of synthetic resins which are used in dentistry as restorative material or adhesives. Synthetic resins evolved as restorative materials since they were insoluble, aesthetic, insensitive to dehydration, easy to manipulate and reasonably inexpensive. Many dentists today use resin fillings instead of amalgam fillings. Composite resins are also used for reshaping teeth, partial crowns, and to adhere retainers.
Read More
Posted by Debbi Cohen on Wed, Jun 01, 2011
1.jpg)
Dental materials ranging from composite resin fillings, to porcelain to metal crowns and bridges, to alginate impression material, to dental adhesives for bonding and restorative dentistry are all tested for their mechanical property strengths. ISO 6872, ISO11405, ISO14801, ISO 9917, and other standards specify the requirements and the corresponding test methods to access dental materials.
Read More
Posted by Nicholas Schaulsohn on Fri, May 13, 2011

Choosing the right testing machine can help lower costs and accelerate product development. Whether company is buying its first testing system or is looking for a different type of system to perform tests on a new product, purchasing a testing system is an important decision. We’ve put together 10 easy steps to help you select the perfect system for your testing application.
Read More
Posted by Nicholas Schaulsohn on Tue, Apr 19, 2011

ASTM D412 (D 412) is the most widely referenced testing standard for measuring the tensile properties of thermoset rubbers and thermoplastic elastomers. ASTM D412 covers two test methods, A and B. The more popular method is A, which can be performed using a universal testing machine also known as a tensile testing machine or tensile tester. This is a general guide intended to help you understand the basic test procedure and the different system configurations you can use to perform this test. When you are ready to test your products or materials to this standard, we recommend purchasing and referencing the official ASTM D412 document.
Read More